METAL TEST COUPONS
Temporary Corrosion Preventive Fluid, Soft Film, Solvent Deposited, Water Displacing | IS 1154 | Annex A : Film thickness MS Panel – IS 513 | 178 | 60 x 80 x 2 (with 50×50 cut-out& Mo holes) | |
Annex B : Drainage Test MS Panel – IS 513 | 179 | 80 x 40 x 1.3 mm with 6 mm hole | |||
Annex E: Water Displacement MS Panel – IS 513 | 180 | 76 x 38 x 1.25 mm in size with 6 mm dia hole | |||
Annex E: Corrosive effect onb Lead Lead (99.9% min.) | 181 | 75 x 50 x 1.5 mm in size | |||
Annex G : Freedom from Corrosive effect | |||||
I) Mild Steel – IS 513 | 182 | 50x25x2to 3 mm in size | |||
ii) Brass – CuZn37 (IS 410) | 183 | 50x25x2to 3 mm in size | |||
iii) Aluminium Alloy – IS 537 | 184 | 50x25x2to 3 mm in size | |||
iv) Magnesium Alloy Ref. 2.1.4 | 185 | 50x25x2to 3 mm in size | |||
v) Zinc Base Alloy – IS 713 | 186 | 50x25x2to 3 mm in size | |||
General purpose oil based temporary corrosion preventives | IS 14779 | Annex A : Film Thickness MS Panel – IS 513 | 187 | 60 x 80 x 2 (with 50×50 cut-out & Mo holes). | |
Turbine oil rust test for corrugated cargoes | ASTM D 665 IS 1448 P:96 NACETM 0172 | Steel specimen (BS970, Part I/SAE 1018) | 188 | 1/2 inch dia, US thread, 81L | |
PTFE holder | 189 | ||||
PTFE beaker cover | 190 | 95.3 dia x 2.4thk | |||
SS stirrer | 191 | 25 x 6 x 0.6thk | |||
Method for corrosion protection test for TCP | IS 10493 | MS (IS 513) | 192 | 100 x 150 , 3mm hole | |
Test for protection against corrosion at high temperature & high humidity(cabinet test) | MS (IS 513) | 193 | 100 x 50 x 2.5 thk | ||
Brass (IS 410) | 194 | 100 x 50 x 2.5 thk | |||
Aluminium alloy (US 713) | 195 | 100 x 50 x 2.5 thk | |||
Test for freedom from corrosive effect on metal specimen | MgAlloy | 196 | 100 x 50 x 2.5 thk | ||
196A | 50 x 25 x 2.5thk | ||||
Zinc base alloy(IS 713) | 197 | 100 x 50 x 2.5 thk | |||
197A | 50 x 25 x 2.5 thk | ||||
Test for corrosion effect on lead strip, copper strip, strippable coatings | Annealed electrolytic Cu (>99.9%) | 198 | 75 x 13 x 2 thk | ||
Lead strip (IS 405) (Part 1) | 199 | 75 x 50 x 1.6thk | |||
Cold finished strip (IS 513) | 200 | 75 x 50 x 2 thk | |||
Sulphur dioxide test(IP Test) | MS (IS 513) | 201 | 150 x 50 x 0.9 thk | ||
Salt spray test | ASTM B 117 | MS panels | 202 | 127 x 76 x 0.8 thk | |
Metal corrosion test | MS sand blasted panels by 50 micron AI sand with 120 degree | 202A | 127 x 76 x 0.8 thk | ||
Metal corrosion test | Mild steel grade NIL 22698 both sides blasted panels with medium grit | 202B | 152 x 106 x 3.2 thk | ||
Cyclic wet/dry prohesion test | ASTM G 85 A5 | MS panels | 203 | 100 x 50 x 2 thk | |
Rust protection by metal preservatives in the humidity cabinet | ASTM D 1748 IP 366 | C.R. ship A 109 or (g9-S-698 Gr 1009) | 204 | 102 x 51 x 3.2 thk (Two holes 3 each) | |
Dummy panel SS 304. | 204A | 102 x 51 x 3.2 thk (Two holes 3 each) | |||
Dummy panel Metha acrylic. | 204B | 102 x 51 x 3.2 thk (Two holes 3 each) |